Inventor: Gsella; Wolfgang
Address: Koln, DE
No. of patents: 2
Patents:
| Patent Number |
Title Of Patent |
Date Issued |
| 7553916 |
Loop reactor with varying diameter for olefin polymerization |
June 30, 2009 |
| Process for polymerizing at least one olefinic monomer in a loop reactor at from 20 to 150.degree. C., but below the melting point of the polymer to be formed, and a pressure of from 5 to 100 bar, where the polymer formed is present in a suspension in a liquid or supercritical suspension |
| 7517938 |
Loop reactor with varying diameter for olefin polymerization |
April 14, 2009 |
| Process for polymerizing at least one olefinic monomer selected from ethylene, propylene and 1-butene in a loop reactor in the presence of a polymerization catalyst at from 20 to 150.degree. C., but below the melting point of a polymer to be formed, and a pressure of from 43 to 80 ba |
|
|
|