Patent Number Title Of Patent Date Issued
7128871 Silver-colored alloy with low percentages of copper and zinc October 31, 2006
A silver-colored, tarnish-resistant, corrosion-resistant alloy is provided. The alloy includes 92.5 95% silver, combined with a master alloy of 24 34% zinc; 60 74% copper; 0.5 1.8% silicon; 0.0 8.0% tin, or 0.0 1.5% indium, wherein percentages are in terms of weight. The alloy can be
5882441 Silver colored alloy with low percentage copper March 16, 1999
A silver colored alloy, highly tarnish resistant, corrosion resistant and brittleness free is provided. The alloy includes 90% to 94% by weight silver, 3.50% to 7.35% by weight zinc, 1% to 3% by weight copper, and 0.1% to 2.5% by weight silicon. The alloy is suitable for rings, earrings,
5817195 Silver colored alloy with low percentage of nickel and copper October 6, 1998
A silver colored alloy highly tarnish resistant, sterling silver is provided or having included therein: 90% to 92.5% by weight Silver; 5.75% to 7.5% by weight Zinc; 0.25% to less than 1% by weight Copper; 0.25% to 0.5% by weight Nickel; 0.1% to 0.25% by weight Silicon; and 0.0% to 0.5%
5019335 Gold colored metal alloy May 28, 1991
The present invention provides an improved casting alloy for use in costume jewelry and jewelry samples. In accordance with the present invention, a gold colored metal alloy is disclosed which is tarnish resistant and consists of the following ingredients such as, 75 to 85% copper, 5 to
4948557 Tarnish resistant gold colored alloy with enhanced gold color August 14, 1990
A gold colored, tarnish and corrosion resistant alloy is disclosed, usable for jewelry, dental purposes and the like. The alloy consists essentially of 24 to 27 percent palladium, 19 to 22 percent indium, 5 to 30 percent copper, 1 to 20 percent gold, and the balance is essentially silver
4895701 Gold colored alloy composition with zero percent gold January 23, 1990
A gold colored, tarnish and corrosion resistant gold free alloy is disclosed, usable for jewelry, dental purposes and the like. The alloy consists essentially of 24 to 27 percent palladium, 19 to 22 percent indium, 5 to 30 percent copper, and the balance is essentially silver.
4865809 Copper-free gold alloy composition September 12, 1989
A gold colored, tarnish and corrosion resistant copper free allow is disclosed usable for jewelry, dental purposes and the like. The alloy consists essentially of 8 to 20 percent Gold, 22 to 26 percent Indium, 22 to 28 percent Palladium, and the balance is essentially Silver.










 
 
  Recently Added Patents
Image processing apparatus and method configured to calculate defocus amount of designated area
Wireless communication apparatus, a method of wireless communication, and a program for wireless communication
Field device configuration system
Providing user interfaces and window previews for hosted applications
Tint block image generation program and tint block image generation device
Memory controller including a hardware compression and decompression engine for managing system memory and graphical operations
Transcription factor
  Randomly Featured Patents
Rotary paper cutter construction
Hinged vehicle gate arm
Self-locking preload controlling nut
Curable coating compositions having improved effect pigment orientation and a method of using the same
Magnetic resonance imaging apparatus in which a rotating field is generated and detected
Optical fiber module with surface emitting laser
Process for the preparation of cyanogen chloride
Pepper mill
Method of extracting parasitic capacitance values from the physical design of an integrated circuit
Urine collection device