Low defect density diamond single crystal and a process for the production of the same

Image Number 2 for United States Patent #5908503.

A colorless, transparent low defect density, synthetic type IIa diamond single crystal, in which the etch pits due to needle-shaped defects are at most 3.times.10.sup.5 pieces/cm.sup.2, and which can be applied to uses needing high crystallinity of diamond, for example, monochromators, semiconductor substrates, spectroscopic crystals in X-ray range, electronic materials, etc., is provided by a process for the production of the colorless, transparent low defect density, synthetic diamond single crystal by growing new diamond crystal on a seed crystal of diamond by the temperature gradient method which comprises using a crystal defect-free diamond single crystal, as a seed crystal of diamond, and optionally subjecting to a heat treatment in a non-oxidizing atmosphere at a low pressure and a temperature of 1100 to C.

  Recently Added Patents
Electric separator, method for the production and use thereof
Clothing fastener accessory
Wristband with detachable labels
Phospholipid-based powders for drug delivery
Display device and method of manufacturing the same
SONOS stack with split nitride memory layer
Case for electronic device
  Randomly Featured Patents
Optical link module, optical interconnection method, information processor including the optical link module, signal transfer method, prism and method of manufacturing the prism
Floating type analog-to-digital converter using delay units to achieve a wide dynamic range
Memory system and method for providing error correction
Disk array system
Obstacle detection system for underground operations
Apparatus and method for measuring heart rate
Microwatt thermoelectric generator
Folding escape/rescue ladder
Brake positioning system
Prosthetic implant cement deflector system