Name: Metal treatment > Process of modifying or maintaining internal physical structure (i.e., microstructure) or chemical properties of metal, process of reactive coating of metal and process of chemical-heat removing (e.g., flame-cutting, etc.) or burning of metal > Producing or treating layered, bonded, welded, or mechanically engaged article or stock as a final product > Utilizing wave energy (e.g., laser, electromagnetic wave energy, etc.), plasma or electron arc or beam
Description: Process which utilizes wave energy (e.g., laser, electromagnetic wave energy, etc.), plasma or an electron arc or beam for (1) modifying or maintaining the internal physical structure (i.e., microstructure) or chemical properties of metal or a metal alloy or (2) in a combined process that includes a step of modifying or maintaining the internal physical structure or chemical properties of metal or a metal alloy, the use of electromagnetic wave energy, plasma, electron arc or beam for any purpose.
Patents under this class:
| Patent Number |
Title Of Patent |
Date Issued |
| 7587818 |
Repair of gas turbine blade tip without recoating the repaired blade tip |
Sep. 15, 2009 |
| 7586061 |
Method of controlled remelting of or laser metal forming on the surface of an article |
Sep. 8, 2009 |
| 7540930 |
Stent to be implanted in human body and method of producing stent |
Jun. 2, 2009 |
| 7537664 |
Laser-produced porous surface |
May. 26, 2009 |
| 7491449 |
Copper-silver alloy wire and method for manufacturing the same |
Feb. 17, 2009 |
| 7470335 |
Method of modifying a workpiece following laser shock processing |
Dec. 30, 2008 |
| 7455740 |
Method for producing a three-dimensional moulded body |
Nov. 25, 2008 |
| 7344609 |
Ultrasonic impact methods for treatment of welded structures |
Mar. 18, 2008 |
| 7322396 |
Weld closure of through-holes in a nickel-base superalloy hollow airfoil |
Jan. 29, 2008 |
| 7235144 |
Method for the formation of a high-strength and wear-resistant composite layer |
Jun. 26, 2007 |
| 7214280 |
Plasma-assisted decrystallization |
May. 8, 2007 |
| 7168160 |
Method for mounting and heating a plurality of microelectronic components |
Jan. 30, 2007 |
| 7166175 |
Method and device for hardening a metal component by plasma pulse technology |
Jan. 23, 2007 |
| 7140216 |
laser aligned shotpeen nozzle |
Nov. 28, 2006 |
| 7067022 |
Method for protecting a surface |
Jun. 27, 2006 |
| 7067021 |
Method of manufacturing multilayer material for plain bearing |
Jun. 27, 2006 |
| 7063896 |
Metallic surface of a body, method for producing a structured metallic surface of a body and the use thereof |
Jun. 20, 2006 |
| 7001672 |
Laser based metal deposition of implant structures |
Feb. 21, 2006 |
| 6972058 |
Heat treatment method and apparatus |
Dec. 6, 2005 |
| 6972390 |
Multi-laser beam welding high strength superalloys |
Dec. 6, 2005 |
| 6962025 |
Metal plasma surface-modified thermal barrier channel |
Nov. 8, 2005 |
| 6936118 |
Process of forming a composite coating on a substrate |
Aug. 30, 2005 |
| 6923877 |
Method and apparatus for improving material properties |
Aug. 2, 2005 |
| 6881282 |
Method of manufacturing a chromed bumper |
Apr. 19, 2005 |
| 6872912 |
Welding single crystal articles |
Mar. 29, 2005 |
| 6852179 |
Method of modifying a workpiece following laser shock processing |
Feb. 8, 2005 |
| 6843866 |
Process for producing wear-resistant surface layers |
Jan. 18, 2005 |
| 6821362 |
Manufacturing method of auger |
Nov. 23, 2004 |
| 6805970 |
Laser peening of components of thin cross-section |
Oct. 19, 2004 |
| 6800149 |
Tapered corrosion protection of tubes at mud drum location |
Oct. 5, 2004 |
| 6767419 |
Methods of forming hardened surfaces |
Jul. 27, 2004 |
| 6743310 |
Method of forming nitride capped Cu lines with improved adhesion and reduced electromigration along the Cu/nitride interface |
Jun. 1, 2004 |
| 6677037 |
Laser shock peening tape, method and article |
Jan. 13, 2004 |
| 6673169 |
Method and apparatus for repairing superalloy components |
Jan. 6, 2004 |
| 6652677 |
Process of welding gamma prime-strengthened nickel-base superalloys |
Nov. 25, 2003 |
| 6610154 |
Surface treatment of austenitic Ni-Fe-Cr based alloys for improved resistance to intergranular corrosion and intergranular cracking |
Aug. 26, 2003 |
| 6589364 |
Formation of doped silicon-germanium alloy utilizing laser crystallization |
Jul. 8, 2003 |
| 6570126 |
Simultaneous offset dual sided laser shock peening using low energy laser beams |
May. 27, 2003 |
| 6558485 |
Laser shock peening with an explosive coating |
May. 6, 2003 |
| 6554924 |
Metallic diffusion process and improved article produced thereby |
Apr. 29, 2003 |
| 6548125 |
Method of internally coating a weapon barrel by means of a laser beam |
Apr. 15, 2003 |
| 6549602 |
Incore piping section maintenance system of reactor |
Apr. 15, 2003 |
| 6534134 |
Apparatus and method for pulsed laser deposition of materials on wires and pipes |
Mar. 18, 2003 |
| 6527881 |
Method for producing a tin-nickel alloy film |
Mar. 4, 2003 |
| 6528183 |
Clad aluminum alloy sheet for aircraft structural parts |
Mar. 4, 2003 |
| 6511559 |
Process for producing wear-resistant edge layers in precipitation-hardenable materials |
Jan. 28, 2003 |
| 6495793 |
Laser repair method for nickel base superalloys with high gamma prime content |
Dec. 17, 2002 |
| 6489584 |
Room-temperature surface weld repair of nickel-base superalloys having a nil-ductility range |
Dec. 3, 2002 |
| 6486100 |
Method for preparing preferentially oriented, high temperature superconductors using solution reagents |
Nov. 26, 2002 |
| 6479168 |
Alloy based laser welding |
Nov. 12, 2002 |
|
|
|