| 4548794 |
Method of recovering nickel from laterite ores |
October 22, 1985 |
| According to the present invention, processes are provided for recovery of nickel, cobalt and like metal values from laterite ores wherein the ores are separated into high and low magnesium containing fractions, the low magnesium fraction is leached with sulfuric acid at elevated tempera |
| 4541994 |
Method of liberating nickel- and cobalt-enriched fines from laterite |
September 17, 1985 |
| According to the present invention, Ni- and Co-rich, low Mg fines may be advantageously separated from the coarse fractions of lateritic ores by atmospheric or low pressure leaching. In particular, the process of the present invention comprises contacting a lateritic ore or ore fraction |
| 4541868 |
Recovery of nickel and cobalt by controlled sulfuric acid leaching |
September 17, 1985 |